What causes streaking on a tennis court surface?
SportMaster's answer sheet on what causes streaking on a tennis court surface. Excessive streaking, in most cases, is from over dilution of the color coatings beyond the range on the specification sheets and labels. On hot days it advises applying in the morning, above 90 degrees Fahrenheit especially, and misting the surface approximately 3 to 5 feet ahead of the squeegee. Other causes: the wrong squeegee (the sheet recommends a sport squeegee of 50 to 60 durometer rubber), angular instead of rounded sand, and pouring onto the surface instead of into the puddle.
1 page, 934 KB
This is SportMaster's document, kept here so our customers and crews can read it beside our own pages. SportMaster's own copy is on sportmaster.net.
Open the PDF (1 page, 934 KB) Key facts
| Question | What causes streaking on a tennis court surface? |
|---|---|
| Main cause | Over dilution of the color coating materials |
| Hot weather | Above 90 degrees Fahrenheit, schedule applications during the morning |
| Misting | Mist approximately 3 to 5 feet ahead of the squeegee, without puddles |
| Sand | Rounded sand in the color coatings; never playground sand |
Taken from this document. The PDF is SportMaster's official document.
The full text of this document
This is the document's own text, moved from the PDF by machine, word for word, and checked against it. The PDF is SportMaster's official document. If the two ever differ, the PDF is right.
Call Today – (800) 395-7325 · Email: moreinfo@sportmaster.net · www.sportmaster.net · Question: What causes streaking on a tennis court surface?
Answer: There are many variables that may contribute to streaks and splotches on a tennis court surface.
Excessive streaking, in most cases, is from over dilution of the color coating materials. There is an acceptable range of dilution stated on the specification sheets and labels, depending on pavement temperatures. Make sure not to exceed this range, and if needed, wait until cooler periods to apply your next coat. Morning is ideal for application during very hot days. If the ambient temperatures are above 90 degrees Fahrenheit, it may be best to schedule applications during the morning.
Another helpful procedure to minimize streaking, on hot days, is to mist the surface approximately 3 to 5 feet ahead of the squeegee applicator. This helps to drop the surface temperature, minimize coating shock, and slow evaporation of the water (vehicle) in the coatings. The surface can be slightly damp during application of the Acrylic Resurfacer and color coatings, but make sure not to create any puddles.
Here are a few pictures that demonstrate streaking from over dilution:
Other basic items that can contribute to streaks on the surfaces are:
- Using the incorrect tool/squeegee for application.
- o A sport squeegee with 50-60 durometer softness of rubber is ideal for application of acrylic sport surfaces. Rubber blades that are softer can wipe the material off and harder (stiffer) rubber blades can drag the sand through and create more visible streaks. The SportMaster sport squeegee is perfectly designed for applying acrylic coatings with a tapered edge and targeted softness.
- Not using the correct sand in the tennis court surface (color coatings).
- o Rounded sand is recommended in the colored surface coatings. Angular cut sand drags under the application squeegee blade, where rounded sands will “roll” and minimize visible streaking left on the color coating surfaces. Never use “playground” sand. It usually contains small stones and/or dusty sand.
- Utilizing the wrong pouring technique.
- o Pour marks can appear on the surface, even from earlier coats. This can happen when the coatings are poured directly onto the surface and not into an existing puddle. The surface can appear splotchy or even streaky, and highlight each pass of the squeegee.
- Proprietary Formulation.
- o SportMaster is specifically formulated with a proprietary blend to provide a pure, vibrant coating that produces a streak-free finish. If properly diluted, SportMaster will provide a finish without streaking issues known as “bacon stripping” or “highlighting”.
Free estimates
Planning a court or a surface?
Industrial Surface is a SportMaster authorized installer in Northeast Ohio. Send the address and what you have in mind; we walk the site, measure it, and send a written proposal with the scope spelled out.
The yard
4000 East 86th Street, Cleveland, OH 44105
Off Broadway Avenue, south of downtown, ten minutes from I-77 and I-490.
Serving Cuyahoga, Summit, Lake, Lorain, Medina, Geauga, Portage, Stark and Ashtabula counties. Municipal, school, club, HOA and commercial work; residential courts by the job.